CuSo4( copper sulphate ) test is quick check to asses the iron contamination
From: R.Bathula@ticb.com
To: materials-welding@googlegroups.com
Date: Wed, 5 May 2010 00:41:34 -0700
Subject: RE: [MW:5077] Iron contamination
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Wednesday, May 05, 2010 12:20 PM
To: materials-welding@googlegroups.com
Subject: [MW:5076] Iron contamination
Dear Friends
Can anyone explain me the procedure to check " Iron contamination " on SS304L plates..
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9820313278
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Invest your money wisely post Budget Sign up now.
From: R.Bathula@ticb.com
To: materials-welding@googlegroups.com
Date: Wed, 5 May 2010 00:41:34 -0700
Subject: RE: [MW:5077] Iron contamination
Pl refer ASTM A 380 for test methods. such as high humidity, copper sulphate or ferroxyl tests
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Wednesday, May 05, 2010 12:20 PM
To: materials-welding@googlegroups.com
Subject: [MW:5076] Iron contamination
Can anyone explain me the procedure to check " Iron contamination " on SS304L plates..
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9820313278
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Invest your money wisely post Budget Sign up now.
Comments