Hi.....yes the code is Asme B31.4/ .....some of our friend confirm that they used 10% RT for hydrocabons product and no test for waste water, fresh water ...
thanks
regards
On Tue, May 4, 2010 at 7:14 AM, B.Vaithiyanathan <pavainathan@gmail.com> wrote:
--Hi,Let me know your design code whether ASME B 31.4/31.8 then only you can decide on extent of NDT.Since it's a modification work you can check with your client what was the design of code of existing line.Regards,VaithiyanthanQA Engineer,WorleyParsons-Arabian industriesOmanOn Mon, May 3, 2010 at 4:39 PM, daniel iordache <daniel.iordache@gmail.com> wrote:Hello,Our client asked for a modification and implemetation for 4 new pipeline that will transfer products( goasoil, water, waste water) over the jetty to barge.....Anyone that have a previous project like that can help me with procentage of inspection especiially for RT test ....?regards
--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro: +40721731728
E-Mail:daniel.iordache@ao.bureauveritas.com
daniel.iordache@gmail.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
With Best Regards
B.Vaithiyanathan
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro: +40721731728
E-Mail:daniel.iordache@ao.bureauveritas.com
daniel.iordache@gmail.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
1 comment:
Hi,
Refer ASME B 31.8 Para 826 & 840.22
you will get the requirement of NDT extent.
Vaithiyanathan
Post a Comment