Monday, May 3, 2010

Re: [MW:5017] A number

Hi,
 
A number means the chemical composition of filler metal. Same as P number, to
reduce the number of PQRs ASME  Sec IX grouped the filler metal with A numbers.
A number is essential variable. If any change in A number it calls for new procedure qualification. We can use different AWS classification with same A number according to the applicability without new qualification of PQR.
 
Regards,
Ibrahim
 
On 3 May 2010 09:45, arijoy roy <bhaitu1@yahoo.com> wrote:
Dear
Please explain to me the significance of the A number mentioned in ASME Sec-IX
With Regards
Arijoy Roy
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...