Monday, May 3, 2010

Re: [MW:5011] Increasing the mechanical sternght by Quenching and tempering.

Hi,
 
Please note that only with heat treatment you cannot change one material grade to another.
The elements added in the material, manufacturing methode & heat treatment are togrther plays the role in the strength of material.
 
It  means for X65 pipe you have to buy X65 pipe or multiple certified pipe in which manufacture guarantee the property of X65 pipe.
 
Regards,
 
Ibrahim 

On 2 May 2010 10:53, Moen - QA <Syed.Moin@gerabgroup.com> wrote:

Dear All,

Can any body guide me on how to increase the mechanical strength of an X52 or X60 pipe?

We want to perform a quenching and tempering heat treatment on pipe of Grade X52 and X60 in order to achieve a mechanical strength equal to the X65 pipe.

I am not familiar with this process, appreciate if anyone can answer to the below question,

1)      Is it possible to enhance the mechanical properties by QT?

2)      What should be the quenching and tempering temperatures?

3)      Medium for quenching

4)      Tempering temperature and holding time.

5)      Is there any formula which utilizes the chemical composition to find out the quenching and tempering temperature and holding time etc?

6)      Method of heating.

    If any one has done this before please share you experience.

Thanks & Regards
Syed Moin                               



______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...