Dear All,
We have qualified a single V groove welding procedure in 3G position as per AWS D1.1. With this procedure, i can only do 3G in groove and 3F in Fillet. So i have prepared pre qualified single V groove WPS for groove welding in all positions.
But we have some jobs which demand 1F and 2F positions. So, i want to know whether prequalified WPS for the single V which i made is acceptable for doing fillet welding in all positions?? Or is there any prequalified WPS for fillet available ??
--
Thanks and Regards
Shahul
QC WELDING ENGINEER
CSWIP 3.1, AWS CWI
Aasia Steel Factory Co. Ltd
KSA
We have qualified a single V groove welding procedure in 3G position as per AWS D1.1. With this procedure, i can only do 3G in groove and 3F in Fillet. So i have prepared pre qualified single V groove WPS for groove welding in all positions.
But we have some jobs which demand 1F and 2F positions. So, i want to know whether prequalified WPS for the single V which i made is acceptable for doing fillet welding in all positions?? Or is there any prequalified WPS for fillet available ??
--
Thanks and Regards
Shahul
QC WELDING ENGINEER
CSWIP 3.1, AWS CWI
Aasia Steel Factory Co. Ltd
KSA
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments
There is not requried any pre qualified WPS for 1F or 2F position. Same 3G WPS u can use for that perticular joint.