some one can help welding overlay with ss for carbon steel cladded vessel (sa516gr70/ss316l)

process : saw


ganesh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

Unknown said...

Weld overlay procedure can be qualified as per ASME SEC-IX and for Overlay nowhere SAW process is followed either GTAW or SMAW is followed