Re: [MW:4849] RE: 4827] cellulose electrodes.

Cellulose electrodes are good for vertical down welding.
- Deep penetrating welding in every position,
- Vertical down welding capability,
- Weld metal with good mechanical properties.

Cellulosic manual electrodes with vertical-down progression has been used for decades. It offers fast travel speeds and can accommodate poor fit-up.

  • Pipe strength: While cellulosic electrodes are suitable for low strength pipe, higher strength pipe and weld metal require low hydrogen electrodes to minimize cracking.
  • However, past experience has shown that high strength steel pipe can be successfully welded using a cellulosic root and hot pass with proper preheat and filling the remainder of the joint with a low hydrogen electrode.



  • disadvantage

    However, there main drawbacks:
    1) It leaves deep undercut grooves along the edges of the weld face, commonly referred to as wagon tracks; and
     2) it usually is necessary to expose these wagon tracks so they can be consumed by the next weld pass — the "hot" pass. This is done by removing the weld crown by grinding.
    3)Thus, using cellulosic electrodes requires extra time after welding the root pass to remove part of the weld and then replace this with new weld metal.
    4) Also, cellulosic electrodes produce weld metal with relatively high levels of weld diffusible hydrogen, rendering it crack sensitive when used on higher strength pipe grades.
    welding.Its drawbacks 
    5) Diffusible hydrogen: Some requirements specify only electrodes that meet a certain maximum weld metal diffusible hydrogen level may be used. In these cases, cellulosic electrodes are usually prohibited.
    6)This increase in strength has caused some issues, especially when using cellulosic electrodes which are sensitive to cracking on higher strength steels. It is usually recommended to weld high strength steel with low hydrogen electrode for all passes


     
    On Wed, Apr 14, 2010 at 7:51 PM, John Henning <jhenning@deltak.com> wrote:
    The primary advantage to cellulose electrodes (EXX10 and EXX11) is that they form a thin slag cover and are what Lincoln electric called "fast freeze".  They produce a deeply penetrating arc but because of the thin slag, solidify rapidily.  Therefore they are very good at bridging gaps and were used for making root passes in piping/pipe lines.
     
    The major disadvantage is that the cellulose, a hydrocarbon, breaks down in the heat of the arc and produces copious hydrogen which is absorbed into the molten weld pool.  These electrodes produce the highest weld metal hydrogen of all common practices/processes.  Therefore they may cause hydrogen assisted cracking if the other required factors are present.   
     
    A minor disadvantage is that the weld is coarse in appearance due to the high solidification rate and therefore may lack visual appeal.
     
    John


    From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prashant pansare
    Sent: Wednesday, April 14, 2010 8:55 AM
    To: mat wel
    Subject: [MW:4827] cellulose electrodes.

    Dear all,
    What r advantages & dis-advantages of cellulose electrodes.
    Pl. reply.
    psp

    --
    To post to this group, send email to materials-welding@googlegroups.com
    To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
    For more options, visit this group's bolg at http://materials-welding.blogspot.com/
    The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

    --
    To post to this group, send email to materials-welding@googlegroups.com
    To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
    For more options, visit this group's bolg at http://materials-welding.blogspot.com/
    The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



    --
    Yadav Shiva Chelliya,
    Inspection Engineer,
    Doha Qatar,
    +974-6166465

    --
    To post to this group, send email to materials-welding@googlegroups.com
    To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
    For more options, visit this group's bolg at http://materials-welding.blogspot.com/
    The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

    Comments

    Popular posts from this blog

    Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

    Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

    Materails FAQs

    Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

    Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

    Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...