Clint specification is the first requirements of the application, even though in general
GTAW cr-mo, Purging root weld quality will   be    achieve  uniform very smooth counter penetration,
 regards
N.Devan
 
On 4/15/10, qaqcmpm <mamujeebali@gmail.com> wrote:
One of our client specn asks for argon purging of root pass (pressure
retaining welds) for GTAW for Low alloy Cr-Mo steel? why it is
required any idea?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe, reply using "remove me" as the subject.



--
Natarajan.Devan
Senior Welding Inspector
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385

INDIA: 0091 9840330143 Res.
Mobile: 0091 9884745254

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...