Dear Sir,
 
UCS 67 (a) (2) says 'Weld made with filler metal shall be impact tested if base metal is excempted by UCS 66 and MDMT is colder than-29 deg.c and not colder than-48deg.c and welding consumable is classified by impact test at a temperature not warmer than the MDMT by the applicable SFA Specification is used.
 
In my case I mentioned ER 70S-3 is specified for -20 deg.C as per SFA Spec. which is warmer than the MDMT of the euipment (-46 deg C).
My query is, as stated in UCS 67 I have Impact tested the PQR at MDMT -46 and passed the test. As per the proven support of PQR can I use ER 70 S3 for -46 deg.C application without seperate batch test?.
 
Regards,
Muhammed Ibrahim PK


 
On 2 April 2010 18:13, <george.dilintas@gr.bureauveritas.com> wrote:

Then you will find your answer in USC-67.
If you do not have the code or you have interpretation problems let me know.


  From: Muhammed Ibrahim [ibratech@gmail.com]
  Sent: 02/04/2010 16:34 ZE4

  To: materials-welding@googlegroups.com
  Subject: Re: [MW:4670] ER70S-3 for low temperature application


Hi,
 
The code is ASME SEC. VIII Div.1.
 
Regards,
Ibrahim


 
On 2 April 2010 09:58, <george.dilintas@gr.bureauveritas.com> wrote:

Could you clarify what is the application code? Section I, section VIII-1?


  From: Muhammed Ibrahim [ibratech@gmail.com]
  Sent: 01/04/2010 18:40 ZE4

  Subject: [MW:4661] ER70S-3 for low temperature application


Hi members,
 
Please provide a suggestion for the following query.
 
I have qualified a PQR for GTAW+SMAW with ER70S-3 & E7018-1. The PQR is impact tested at - 46 deg C at root(GTAW) and filling (SMAW) and passed (Min. 50J energy obtained).
 
As per ASME Sec.II part C, E7018-1 will support up to - 46 Deg C, but ER70S-3 will support up to - 20 Deg.C only.
 
Since I have proven the toughness through PQR, can I use this PQR for job with impact test requirement of - 46 Deg C, even ER70S-3 does not support for this temperature as per Sec.IIC?.
 
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...