Better u Test ER70-S3 with GTAW separately at minus 46 c and u can be sure on this eventhough code does not call
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
On Sat, Apr 3, 2010 at 12:31 AM, Natarajan Devan <devan1961@gmail.com> wrote:
yes you can apply PQR.Once proven record is available. i think your PQR is LTC ( A333)material.regardsN.Devan
--On 4/1/10, Muhammed Ibrahim <ibratech@gmail.com> wrote:--Hi members,Please provide a suggestion for the following query.I have qualified a PQR for GTAW+SMAW with ER70S-3 & E7018-1. The PQR is impact tested at - 46 deg C at root(GTAW) and filling (SMAW) and passed (Min. 50J energy obtained).As per ASME Sec.II part C, E7018-1 will support up to - 46 Deg C, but ER70S-3 will support up to - 20 Deg.C only.Since I have proven the toughness through PQR, can I use this PQR for job with impact test requirement of - 46 Deg C, even ER70S-3 does not support for this temperature as per Sec.IIC?.
Thanks & Regards
Muhammed Ibrahim PK
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Natarajan.Devan
Senior Welding Inspector
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385
INDIA: 0091 9840330143 Res.
Mobile: 0091 9884745254--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments