Skip to main content

RE: [MW:4500] Why maximum PWHT temp shall be at least 20 °C less than tempering temp.

Remaining austenite, larger grain size

Dr. G. Dilintas
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Inactive hide details for "Girish Shejale" <gshejale@mjbi.com>"Girish Shejale" <gshejale@mjbi.com>


          "Girish Shejale" <gshejale@mjbi.com>
          Sent by: materials-welding@googlegroups.com

          08/03/2010 09:20

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

RE: [MW:4484] Why maximum PWHT temp shall be at least 20 °C less than tempering temp.

Ref


What kind of microstructural transformations are expected here?

Regards,

Girish Shejale
      -----Original Message-----
      From:
      materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of george.dilintas@gr.bureauveritas.com
      Sent:
      Monday, March 08, 2010 10:26 AM
      To:
      materials-welding
      Subject:
      Re: [MW:4473] Why maximum PWHT temp shall be at least 20 °C less than tempering temp.

      The pwht temperature must be lower than the lower transformation temperature in order to avoid microstructure alterations.


      From: "Pradip Patil" [pradipp@godrej.com]
      Sent:
      08/03/2010 11:40 ZE5B
      To:
      <materials-welding@googlegroups.com>
      Subject:
      [MW:4472] Why maximum PWHT temp shall be at least 20°C less than tempering temp.


      Dear Sir,

      Why maximum PWHT temp for CS and Low alloy steel materials shall be at least 20°C less than tempering temp?

      With Regards,
      Pradip Patil.

      ============================================================================================
      This message (including any attachments) contains confidential information and is intended solely for the use of the individual or entity to whom they are addressed. If you are not the intended recipient you are notified that disclosing, copying, distributing or taking any action based on the contents of this information is strictly prohibited. If you have received this email in error please notify mailadm@godrej.com. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of Godrej & Boyce Mfg. Co. Ltd. group of companies. The recipient should check this email and any attachments for the presence of viruses. Godrej & Boyce Mfg. Co. Ltd. group of companies accepts no liability for any damage caused by any virus transmitted by this email.

      Please do not print this e-mail unless you really need to.
      ============================================================================================

      --
      To post to this group, send email to materials-welding@googlegroups.com
      To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
      For more options, visit this group's bolg at
      http://materials-welding.blogspot.com/
      The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

      --
      To post to this group, send email to materials-welding@googlegroups.com
      To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
      For more options, visit this group's bolg at
      http://materials-welding.blogspot.com/
      The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

The information contained in this e-mail and any attachments is strictly confidential and is intended for the addressee only. Access to this e-mail by any other person is unauthorised. If you are not the intended recipient please destroy this message, delete any copies held on your systems and notify the originator immediately by reply e-mail. The unauthorised use, disclosure, alteration, copying, distribution or any action taken or omitted to be taken in reliance of this e-mail is strictly prohibited and may be unlawful. Opinions and views expressed in this e-mail are those of the sender. They may not reflect the opinions of MJB International / Masaood John Brown Limited and shall be understood as being neither given nor endorsed by it.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...