Re: [MW:4419] WPS

I would suggest to read carefully the QW 407.1
Many people think that if a WPS is qualified without PWHT is then qualified also with PWHT.
However this is wrong

Dr. G. Dilintas
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Inactive hide details for "Kamalaksha, Arekere" <arekere.kamalaksha@gl-group.com>"Kamalaksha, Arekere" <arekere.kamalaksha@gl-group.com>


          "Kamalaksha, Arekere" <arekere.kamalaksha@gl-group.com>
          Sent by: materials-welding@googlegroups.com

          04/03/2010 05:30

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

[MW:4412] WPS

Ref


Dear all ,

If we qualify the welding procedure for the P1 materials  with post weld heat treatment then whether it is applicable for the welding without post weld heat treatment ,
Please note that here thickness is not the criteria .Post weld heat treatment is required for some of the process line in Refinery.
Please clarify.

Kamalaksh. A
GLIS  GmbH -India
Mobile: +919741506305
Email : kare@gl-group.com
Website: www.gl-group.com



 
--------------------------------------------------------
Please note: New address of GL Head Office in Hamburg as of March 8, 2010

Germanischer Lloyd
Brooktorkai 18
20457 Hamburg / Germany

Phone and fax numbers as well as e-mail addresses will remain unchanged.

Relocation of GL's Head Office in Hamburg starts mid of February 2010.
--------------------------------------------------------

This e-mail and any attachment thereto may contain confidential information and/or information protected by intellectual property rights for the exclusive attention of the intended addressees named above. Any access of third parties to this e-mail is unauthorised. Any use of this e-mail by unintended recipients such as total or partial copying, distribution, disclosure etc. is prohibited and may be unlawful. When addressed to our clients the content of this e-mail is subject to the General Terms and Conditions of GL's Group of Companies applicable at the date of this e-mail.


If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.

GL's Group of Companies does not warrant and/or guarantee that this message at the moment of receipt is authentic, correct and its communication free of errors, interruption etc.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...