you need qualify new PQR using this material. any way pl post the data sheet of this material or check any where it refers to any ASTM/EN/JIS standard


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nitesh Patel
Sent: Friday, February 05, 2010 12:14 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4221] P-NO and F- NO of SUMITON 610 F TMCP Plates

 But as per ASME SEC IX it is mandatory while you prepare WPS.
 

On Fri, Feb 5, 2010 at 11:35 AM, Endri Prasetyo <endri.prasetyo@gmail.com> wrote:
Dear Nitesh,
 
If you cannot find any P and F no with refer to code, just ignore the column for it in WPS form.
Not all materials have that number.
 
regards,
Endri

On Fri, Feb 5, 2010 at 12:54 PM, Nitesh Patel <nitesh.patel2@gmail.com> wrote:
Dear friends,

              I have to weld this material but problem is that for WPS i am not getting the P-No and F- no  for this material.
if anyone know the p-no and f-no for this material

--
With Regards
Nitesh Patel
SGS INDA PVT LTD
+918128407488
+919687206278


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...