Re: [MW:4200] ...can be designed in accordence with API 650...?

you can also consult the book PRESSURE VESSEL HANDBOOK by MAggosy

it had detailed description from dish end to supports emphasizing on
ACSE ASME standards

On 2/3/10, K.M Hrishikesan <hrishikm07@gmail.com> wrote:
> Hi Manohar
>
> API 650 tanks are generally for storage service at atmospheric pressure.
> Also the bottom of the API 650 tanks are uniformly and fully supported.Hence
> not applicable in this case.
> In your case it is an agitated vessel which will have certain amount of
> internal pressure according to the intended service conditions.So this is a
> pressure vessel which can be designed as per ASME section VIII div I with
> special process design of agitator assembly. Leg supports with lugs can be
> designed as per the methods described in process equipment design books such
> as *Brownell&Young.*
> The entire design of the vessel can be performed using design softwares such
> as PVelite.
>
> Regards
>
> Hrishikesan
>
> On Wed, Feb 3, 2010 at 4:25 PM, manohar matcha
> <matchamano@rediffmail.com>wrote:
>
>> Dear members,
>>
>> Following situation/type of tank can be designed inaccordance with API
>> 650...?
>>
>> *situation:*
>>
>> - Vertical cylindrical shell, dia 2650mm
>> - height, 3500mm
>> - tank bottom: 2:1 ellipsoidal dished head
>> - tank top: flat closing (stiffners welded from inside surface) - plate
>> welded to shell (on top plate agitator arrangement will be mounted)
>> - tank supported by 04 legs
>>
>> if not API 650, inaccordance with which code/standard this tank can be
>> designed?
>>
>> Please advise/share your views.
>>
>>
>> Regards,
>> Manohar.
>>
>>
>> <http://sigads.rediff.com/RealMedia/ads/click_nx.ads/www.rediffmail.com/signatureline.htm@Middle?>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding-unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...