Hi Nitesh,

 

TMCP steel is fairly new to ASME boiler and pressure vessel code. If I remember correctly 2007 version of ASME Sec- II Part –C , incorporated this material and till date Sec-IX have not assigned any P No or S-No to this type of steel. Only SA-841-SA-841M Specification for Steel Plates for Pressure Vessels, Produced by Thermo-Mechanical Control Process (TMCP), is included in SEC-II, Pt-A Code.

 

In view of the same as per QW-424 /424.1 this material should be  treated as unassigned material and WPS  and PQR shall be qualified. For unassigned material, ASME recommends to the follow the manufacturer’s guidelines, for welding+ PWHT etc.

 

TMCP steels are popular with offshore codes, it would be a due diligence to cross check the fabrication guidelines of Offshore design codes also for correctness of WPS and PQR. AWS, D-1.1-2004 or 2008  briefly refers  on welding  of TMCP steel.

 

If you could post the data sheet of the material (SUMITON 610 F TMCP Plates), more appropriate suggestions could be provided. I extracted this info from Sumitomo Catalogue, which shows a product SUMITEN-610F. I am not sure if it’s the same steel you’re talking about.

 

Thanks.

 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Engineering & Training Services Division

ONTARIO POWER GENERATION Inc.

PO Box-2000, RR-55(South)

Nanticoke, Ontario,N0A1L0

Tel:-(519) 587-2201, Ext 3107--in Nanticoke

         (416) 231-4111, Ext 5925--in Kipling,Toronto

Fax: (519) 587-6814

Email-pradip.goswami@opg.com.

 

From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Friday, February 05, 2010 6:36 AM
To: GOSWAMI Pradip -THERMAL
Subject: FW: [MW:4222] P-NO and F- NO of

 

 

 

Pradip Goswami

88,Garth Trails Crescent

Hamilton,Ontario, L9B2X1,Canada

Email-pgoswami@sympatico.ca

Email-pgoswami@quickclic.net

Tel-905-679-9677


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Friday, February 05, 2010 2:53 AM
To: materials-welding@googlegroups.com
Subject: RE:
Nitesh

 

you need qualify new PQR using this material. any way pl post the data sheet of this material or check any where it refers to any ASTM/EN/JIS standard

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nitesh Patel
Sent: Friday, February 05, 2010 12:14 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4221] P-NO and F- NO of SUMITON 610 F TMCP Plates

 But as per ASME SEC IX it is mandatory while you prepare WPS.
 

On Fri, Feb 5, 2010 at 11:35 AM, Endri Prasetyo <endri.prasetyo@gmail.com> wrote:

Dear Nitesh,

 

If you cannot find any P and F no with refer to code, just ignore the column for it in WPS form.

Not all materials have that number.

 

regards,

Endri

On Fri, Feb 5, 2010 at 12:54 PM, Nitesh Patel <nitesh.patel2@gmail.com> wrote:

Dear friends,

              I have to weld this material but problem is that for WPS i am not getting the P-No and F- no  for this material.
if anyone know the p-no and f-no for this material

--
With Regards
Nitesh Patel
SGS INDA PVT LTD
+918128407488
+919687206278


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.