Can you give us some more detail on your parameters you were using for
the -5 and the -H4? Are you trying to run the same amps/volts and
travel or have you tried running some different paramters? By the
sounds of it you are using 100% CO2 for the gas. Is that correct?

On Feb 4, 12:43 pm, Elshan Feyzullayev <elsha...@hotmail.com> wrote:
> Dear friends,
>
> I have bought locally AWS A5.20 E70T-5 FCAW wire (ELCOR B70) for welding C-Mn steel.
>
> With this I substituted E71-T1-H4 only for temporary period. But it gives a large amount of spatters during welding. Therefore the welding is somewhere impossible.
>
> best regards
>
> Elshan.
>
> _________________________________________________________________
> Hotmail: Powerful Free email with security by Microsoft.https://signup.live.com/signup.aspx?id=60969

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...