Re: [MW:4158] RE: 4151] RE: 4150] ASME SEC IX...PWHT?

Dear Nandesh,
 
As Per Table - A1, A333gr.6 is exempted from impact testing until -45 Deg.
How there could be an impact requirement @ -21 Deg.C.
 
Can you please clarify.
Thanks and Best regards,
K.Rajagopal
On Thu, Jan 28, 2010 at 9:08 AM, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:
Dear Mr. Pradeep,
 
Yes you are right. Please throw some more light on this issue
 
Material : ASTM A333 Gr. 6
Design code : ASTM B31.3
Service : LNG line
Impact requirement : yes @ -21° C
 
Thanks for the suggestions.
Nandesh

--- On Wed, 27/1/10, pgoswami <pgoswami@quickclic.net> wrote:

From: pgoswami <pgoswami@quickclic.net>
Subject: [MW:4156] RE: 4151] RE: 4150] ASME SEC IX...PWHT?
To: materials-welding@googlegroups.com
Date: Wednesday, 27 January, 2010, 3:48 AM

Nandesh,

 

Looking at your query, if the material of construction is P No/S No-1 then PWHT is mandatory over ¾" or 20 mm pipe wall thickness. This is the PWHT criteria as per B-31.3 -2008 code.

 

If the design code is not B-31.3 then PWHT requirements of the applicable design code will follow. Do you have impact requirements for LNG piping if so @ what temperature?.

 

If you could provide those details e.g. materials grade, SA 333 Gr1 or 6 , design code, design temperature more comprehensive answers could be provided.

 

Thanks

 

Pradip Goswami, P.Eng

88,Garth Trails Crescent

Hamilton,Ontario, L9B2X1,Canada

Email-pgoswami@sympatico.ca

Email-pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandra, Vasanthan (Lagos)
Sent: Tuesday, January 26, 2010 5:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:4151] RE: 4150] ASME SEC IX...PWHT?

 

Nandesh,

 

PWHT requirement is to be cross referred in line with Construction/Design code. In your mail, the applicable design code is missing. However, assuming the design code as B31.3 (2008) for piping, PWHT is mandatory for a thickness >20mm.

 

Regards,
Vasanth

From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of Nandesh Kumar
Sent: 26 January 2010 10:33
To: materials-welding@googlegroups.com
Subject: [MW:4150] ASME SEC IX...PWHT?

 

Dear All,

 

For our LNG piping project, as per ASME SEC IX for a pipe 16 inch OD and Thk 21.44 mm PWHT is manadtory? We are welding root and hot pass TIG and others SMAW.

Material is ASTM A333 .

 

Thaks in advance

Nandesh Kumar A

 


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...