As per ASME code Sec.VIII Div.1,2&3, the same is Category D.
The category tells us about the location of the joint in a pressure vessel. Not the lip type of weld geometry.
Regards,
Raghavendra
The category tells us about the location of the joint in a pressure vessel. Not the lip type of weld geometry.
Regards,
Raghavendra
Larsen & Toubro Limited
www.larsentoubro.com
This Email may contain confidential or privileged information for the intended recipient (s) If you are not the intended recipient, please do not use or disseminate the information, notify the sender and delete it from your system.
>>> romio dabre <romiomdabre@gmail.com> 11/01/2010 01:08 pm >>>
Dear all
What is the joint catagory of LIP type nozzle welded to shell or head? Is it
A or D catagory?
Thks