Tuesday, January 5, 2010

Re: [MW:3978] welding procedure for the material at - 30degree C

HI!
If you maintain the same parameters of the existing procedure, run an additional coupon & impact test at minus 30 degree C & add an addendum to the PQR.
Rgds,
vipin

On Tue, Jan 5, 2010 at 8:57 AM, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
Dear Friends,
 
I have a welding to do on the material where the service temperature is -30 degree C. I have got a welding procedure which charpy V test was carried out at -20 degree C. can I use this procedure for welding of the material which the service temperature is -30 degree C?
 
regards,
Elilk.


Windows Live: Make it easier for your friends to see what you're up to on Facebook.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...