Friday, July 31, 2009

[MW:2856] material specification

Dear Sir,


Please send me EN 8 material properties and ASTM A 668 Material Properties. (Both chemical & mechanical Properties)

Regards

D.Sriram


Looking for local information? Find it on Yahoo! Local http://in.local.yahoo.com/

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2854] Re: 17020 Accreditering - Procedure Requirement

Just inform with third party, ask if they have a checklist availeble to do an assessment yourself?
 

Date: Fri, 31 Jul 2009 09:45:04 +0300
Subject: [MW:2853] 17020 Accreditering - Procedure Requirement
From: erturgut@gmail.com
To: materials-welding@googlegroups.com

Hello,
My company is trying to have ISO 17020 Accreditering
We are aiming to do 2nd and 3rd party inspections, periodic inspections related with API 650 Tanks, API 1104 Pipelines, AD Merkblatter Pressure Vessels, ASME SEC IX Pressure Vessels and some other like these.
Do we have to prepare Procedures, Methods for all of these standards
Or do procedures and methods are needed for non-standard works
Or do we need methods indeed if standards are enough to get the accreditering
 
Thanks in advance
--
Best Regards,

Erhan Turgut
Metallurgical & Materials Engineer
DVS - IIW / EWF International Welding Engineer
EN 473, 97/23/EC PED – UT LII

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2853] 17020 Accreditering - Procedure Requirement

Hello,
My company is trying to have ISO 17020 Accreditering
We are aiming to do 2nd and 3rd party inspections, periodic inspections related with API 650 Tanks, API 1104 Pipelines, AD Merkblatter Pressure Vessels, ASME SEC IX Pressure Vessels and some other like these.
Do we have to prepare Procedures, Methods for all of these standards
Or do procedures and methods are needed for non-standard works
Or do we need methods indeed if standards are enough to get the accreditering
 
Thanks in advance
--
Best Regards,

Erhan Turgut
Metallurgical & Materials Engineer
DVS - IIW / EWF International Welding Engineer
EN 473, 97/23/EC PED – UT LII

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2852] Re: effect of heat treatment on Austentic Steel

Hello Sandeep

Generally ASS are not stress relieved after welding due to the chances of sensitization i.e carbide precipitation in the temperature ranges of 425 - 900 degrees C.
However in certain critical applications for dimensional stability in long service, ASS have to be stress relieved after welding.

We have infact successfully carried out SR of ASS (304LN material)at 400 degreesC and 980 degrees C in certain critical jobs as per client requirement.

Stress relieving at temperatures below 400°C is an acceptable practice but results in only modest stress relief. Stress relieving at 425 to 925°C significantly reduces residual stresses that otherwise might lead to stress corrosion cracking or dimensional instability in service. One hour at 870°C typically relieves about 85% of the residual stresses. However, stress relieving in this temperature range can also precipitate grain boundary carbides, resulting in sensitisation that severely impairs corrosion resistance in many media.
To avoid these effects, it is strongly recommended that a stabilised stainless steel (grade 321 or 347) or an extra-low-carbon type (304L or 316L)or with Nitrogen addition like 304LN be used, particularly when lengthy stress relieving is required.

Full solution treatment (annealing), generally by heating to about 1080°C followed by rapid cooling, removes all residual stresses, but is not a practical treatment for most large or complex fabrications.

Low Temperature Stress Relieving:
When austenitic stainless steels have been cold worked to develop high strength, low temperature stress relieving will increase the proportional limit and yield strength (particularly compressive yield strength). This is a common practice for austenitic stainless steel spring wire. A two hour treatment at 345 to 400°C is normally used; temperatures up to 425°C may be used if resistance to intergranular corrosion is not required for the application. Higher temperatures will reduce strength and sensitise the metal, and generally are not used for stress relieving cold worked products.

Regards

Prem Nautiyal
Godrej, Mumbai.


On Thu, 30 Jul 2009 21:07:01 +0530 wrote
>Can anyone please tell about the effect of effect of heat treatment on
>Austentic Steel?
>
>Regards
>Sandeep kumar
>
>>
>

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Thursday, July 30, 2009

[MW:2851] Re: 2849] effect of heat treatment on Austenitic Steel

 
all about stainless steel.

Effect of austenitic stainless steel composition and heat treatment on cold formability

Introduction

Alloying elements that help stabilize the austenitic phase reduce the tendency of the austenitic stainless steels to work harden. Nickel additions have been used traditionally to do this, but nitrogen also has a profound affect on stability of the austenite phase.

Deep drawing compositions

The nickel level was increased in the superseded BS1449 grade 304S16 compared to the 304S15 level (around 8.0%). This enabled the 304S16 grade with around 8.5% nickel to be used for deep drawing applications. Both these grades are covered in BS EN 10088-2 as 1.4301, but the higher nickel variant can be specified as a 'deep drawing' grade. In contrast the higher nickel variants of 316 (1.4435) were developed for improved 'selective' corrosion resistance, originally in pharmaceutical applications, from lower ferrite levels. The 'standard' 316 type (1.4401) with around 11% nickel should be suitable for deep drawing.

The BS1449 grade 305S19 with its 11.0 - 13.0 % nickel range is even more stable when cold worked. One application for this grade is for temper rolled strip for springs where low magnetic permeability is required. BS EN 10088-2 covers this grade as 1.4303. An alternative is the Sandvik strip grade '13RM19' with 6% manganese and 0.25% nitrogen in addition to 7% nickel.

Stretch forming compositions

Stretch forming application grades would normally have 'standard' nickel levels (around 8.0 / 8.2%), but if the sheet is intended for stretch forming the manufacturer / supplier should be informed, as the final heat treatment / process line speed conditions are adjusted to optimize the mechanical properties. The grain size of cold rolled stainless steel sheet is usually fine enough (around ASTM 7-8) to avoid 'orange peel' surface roughening during pressing.

Effect of cold work and heat treatment on the magnetic permeability of austenitic stainless steels

Introduction

Austenitic stainless steels are generally non-magnetic with magnetic permeabilities of around 1.0. Permeabilities above 1.0 are associated with the amount of either ferrite or martensite phases present in the 'austenitic' steel and so depend on:

  • cold working and heat treatment conditions
  • composition effects

This article discusses the effects of cold working and heat treatment.

Cold working and heat treatment

Cold working of austenitic stainless steels can partially transform austenite to martensite. As martensite is ferromagnetic, cold worked austenitic stainless steels can show a degree of 'pull' towards a magnet. This usually occurs at sharp corners, sheared edges or machined surfaces but can be detected on wrought products such as rods or bars which may have been cold straightened, following the final hot rolling or annealing in the mill.

The degree to which this occurs depends on the compositional effects of austenite stabilising elements. High nickel or nitrogen bearing grades tolerate more cold working before localised increases in permeability are noticed.

These increases in permeability can be reversed by full solution annealing (at temperatures around 1050 / 1120 °C with rapid cooling). This transforms any cold-formed martensite back to austenite, the non-magnetic phase, which is then retained on cooling.

The best austenitic stainless steel types for low permeability applications are those with high austenite stability as these have low permeability in both annealed or cold worked conditions. These include the nitrogen bearing types, 304LN (1.4311) and 316LN (1.4406) or the high nickel types such as 310 (1.4845).

arun

On Thu, Jul 30, 2009 at 7:48 PM, Shahid, Iqbal <Iqbal.Shahid@buthermotech.ca> wrote:

Austenitic steels are referred as non-heattreable in conventional sense i.e. they can't be hardened by transformation hardening mechanism (quench & temper)

The only suitable method to increase strength/ hardness of austenitic grades is cold working.

 

In limited uses a surface treatment such as nitriding can also be tried but at the loss of corrosion resistance, however.

Following heat treatments apply to Austenitic grades:

Solution heat treatment

Stress relieving

Best Regards,

Iqbal 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandy kumar
Sent: July 30, 2009 3:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:2849] effect of heat treatment on Austentic Steel

 

Can anyone please tell about the effect of effect of heat treatment on Austentic Steel?

 

Regards

Sandeep kumar







--
ARUNVANI

Whatever happened - happened for good; Whatever is happening - is happening for good; Whatever will happen - will happen for good. Do not worry about the past or the future - live in the present.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2850] RE: 2849] effect of heat treatment on Austenitic Steel

Austenitic steels are referred as non-heattreable in conventional sense i.e. they can’t be hardened by transformation hardening mechanism (quench & temper)

The only suitable method to increase strength/ hardness of austenitic grades is cold working.

 

In limited uses a surface treatment such as nitriding can also be tried but at the loss of corrosion resistance, however.

Following heat treatments apply to Austenitic grades:

Solution heat treatment

Stress relieving

Best Regards,

Iqbal 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sandy kumar
Sent: July 30, 2009 3:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:2849] effect of heat treatment on Austentic Steel

 

Can anyone please tell about the effect of effect of heat treatment on Austentic Steel?

 

Regards

Sandeep kumar



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2849] effect of heat treatment on Austentic Steel

Can anyone please tell about the effect of effect of heat treatment on Austentic Steel?
 
Regards
Sandeep kumar

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2848] RE: 2847] Tests required on A350LF2 to use temp. for gas / ambient temperature -(minus)40 Deg C

We should always specify the class also; A350 LF2 Class 1 fittings are factory tested at -45.6 °C, unless otherwise specified for lower temperatures, where as A350 class 2 fittings are recommended for up to -18 °C only.

A350 LF2 Class 1 fitting can be used depending on your design temperature (please check MDMT, and not process/operating temp)

CVN impact testing requirement and energy values shall be as per the design code or contract specifications, whichever is stringent, for e.g. B31.3 refer para 323.2.2.

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Velu
Sent: Thursday, July 30, 2009 8:37 AM
To: Materials & Welding
Cc: gr_velu@yahoo.co.in
Subject: [MW:2847] Tests required on A350LF2 to use temp. for gas / ambient temperature -(minus)40 Deg C


HI,

I would like to know whether material A350LF2 can be used for
process / ambient temperature of -40 to 50 Deg C. If yes, what are the
testing required to be carried out to ensure that the valve and other
fittings perform well for this temperature.

I know LTCS A350LF2 is the right choice but the package supplier is
not able to supply valve body with LTCS A350LF2 and he can only supply
with A350LF2.


Thanks in advance

Velu


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2847] Tests required on A350LF2 to use temp. for gas / ambient temperature -(minus)40 Deg C

HI,

I would like to know whether material A350LF2 can be used for
process / ambient temperature of -40 to 50 Deg C. If yes, what are the
testing required to be carried out to ensure that the valve and other
fittings perform well for this temperature.

I know LTCS A350LF2 is the right choice but the package supplier is
not able to supply valve body with LTCS A350LF2 and he can only supply
with A350LF2.


Thanks in advance

Velu

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Wednesday, July 29, 2009

[MW:2845] Re: NACE compliant materail


HI,
     If the H2S increses then heavy corrosion will start , the material used will corrode very fast, maily valves, elbows, fittings... etc. weld joints etc.... The entire system can fail within a year or 6 months ....
On Wed, Jul 29, 2009 at 2:34 PM, Yadav Shiva <luvshiv2002@gmail.com> wrote:
Hi Srini,
               Use material with 18% Cr. for existing facilities, the problem is with client . You just go according to your requirment meets the NACE std. Dont worry about if it exceeds 10% or 20%........ if you wana to become scientest then its your coice.... enjoy.........
 
Y.C.Shiva,
QA/QC Engineer,
Doha Qatar.

On Tue, Jul 28, 2009 at 2:25 PM, Hari Srinivasa Murthy <harimurthy@gmail.com> wrote:
An Oil and Gas exploration gas processing facility has been designed for 3% H2S in the gas (NACE compliant material used in the existing facility). As we cannot predict the behavious of oil wells some times H2S content may increase. 
 
Please putdown your opinions on what could be the various implecations to plant equipment (materials)  if the H2S % raises to 8% or 9%. 
 
Regards
 
Srinivas 





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2844] Re: NACE compliant materail

Hi Srini,
               Use material with 18% Cr. for existing facilities, the problem is with client . You just go according to your requirment meets the NACE std. Dont worry about if it exceeds 10% or 20%........ if you wana to become scientest then its your coice.... enjoy.........
 
Y.C.Shiva,
QA/QC Engineer,
Doha Qatar.

On Tue, Jul 28, 2009 at 2:25 PM, Hari Srinivasa Murthy <harimurthy@gmail.com> wrote:
An Oil and Gas exploration gas processing facility has been designed for 3% H2S in the gas (NACE compliant material used in the existing facility). As we cannot predict the behavious of oil wells some times H2S content may increase. 
 
Please putdown your opinions on what could be the various implecations to plant equipment (materials)  if the H2S % raises to 8% or 9%. 
 
Regards
 
Srinivas 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2846] Bolt Torqueing values

i m working on a project of Bulk Plant.There for underground lines we use RTR(Reinforcement Thermosetting Resins) pipe.and i use Flat Face Flange of RTR.Line Pressure is 150-200 PSI.I use rubber gasket between the Flage Joint.
Also i make spols of CS pipe.There i use RF Flange.
can some one provide me the Table of Torque Values for bolting?
 
Regards,
waqas

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2843] RE: 2839] Re: AWS-CWI best agency in INDIA

Can you please give the address and contact numbers for IANT ( Institute of Advanced NDT Technology)?

 

 

Regards

 

Chandulal S Vithlani

--------------------------------------------------------------------

Dear Prem,
I suggest you that if you are planning to attend AWS for Overseas job opportunities then please think about CSWIP 3.1 welding Inspector.
main difference : AWS validity - 3 years.
                         CSWIP 3.1 - Validity 5 years
AWS membership compulsory. every year you have to pay.
CSWIP membership not compulsory.
Renewal - AWS = INR 22000/- after three years CSWIP 3.1 = INR 15,000/-

Choice is yours! - CSWIP 3.1 = Tata Projects limited.
and for Preparatory courses IANT ( Institute of Advanced NDT Technology)

Regards,
Nilesh

On Tue, Jul 28, 2009 at 4:33 AM, PREMSHANKARDUTTNAUTIYAL <prem_nautiyal@rediffmail.com> wrote:

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278

 




--
Best Regards,

Nilesh Pathare


**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar® technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouge's state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Tuesday, July 28, 2009

[MW:2842] QUERY ON SUITABLE FILLER WIRE FOR INCONEL 600

REPLY DTD 28TH JULY 2009

DEAR SORIN STEFAN
YOU CAN USE AWS ERNiCr-3 GRADE (BRAND OF SPECIAL METALS IS INCONEL
82) FILLER WIRE. AVAILABLE FOR MIG/TIG AND ALSO SAW APPLICATION.
FOR WELDING GUIDELINES VISIT www.specialmetalswelding.com
THIS SITE HAS ALL THE INFO YOU WANT.
REGARDS

CHANDER C GIROTRA
MUMBAI/ INDIA
====================================================
On Jul 24, 7:36 pm, sorin stefan <ssori...@hotmail.com> wrote:
> Hi Guys,
>
> Please tell me what is the best match of the filer material and gas for welding ALLOY 600 ( plates 1/4"up to3/") using MIG and TIG procedures.
>
> If you also have some welding giudelines - welding procedure regardless, it will be great
>
> Getting an answer ASAP it will be very much apreciated
>
> Thanks a lot
>
> Sorin St.
>
> _________________________________________________________________
> Stay on top of things, check email from other accounts!http://go.microsoft.com/?linkid=9671355

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2841] NACE compliant materail

An Oil and Gas exploration gas processing facility has been designed for 3% H2S in the gas (NACE compliant material used in the existing facility). As we cannot predict the behavious of oil wells some times H2S content may increase. 
 
Please putdown your opinions on what could be the various implecations to plant equipment (materials)  if the H2S % raises to 8% or 9%. 
 
Regards
 
Srinivas 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2840] Re: AWS-CWI best agency in INDIA

These days All are more interested in TWI cswip 3.1 /3.2 certification rather than AWS CWI .

These are only a passport for Jobs in Gulf . Even BHEL WRI is best in context to Indian scenario

Best Regards,


----- Original Message -----
From: PREMSHANKARDUTTNAUTIYAL
To: materials-welding@googlegroups.com
Sent: Tue, 28 Jul 2009 09:03:56 +0530 (IST)
Subject: [MW:2827] AWS-CWI best agency in INDIA

Hi Friends



I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .



1)Industrial Quality Concepts

Address: IQC Training & Services, Pte, Ltd

Shivani Block -1, Ist Floor

40 East Coast Road

Chennai, India 600041

Telephone: 91-44-42158714/42158715/24451009

Fax Number: 91-44-5215-8715

Email: iqc.in.org@vsnl.com

Contacts: Sundaran Baskaran



2)BETZ Engineering & Technology Zone

Address: 49-Vellalar Street

Near St Thomas Mount Railway Station

Chennai - 600088

INDIA

Tel: 91-44-65364123/22441234

TeleFax: 91-44-22441234

Email: betzzone@vsnl.net

Site: www.betzinternational.com



3)DASH Inspectorate

Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,

Saffron Circle,Fatehgunj,

Baroda-390002,Gujarat,India

Phone: +91 265 2750116, 3017474

Fax: +91 265 2788278

Site: www.dashinspectorate.com



4)Agency: Moody ICL Certifications Limited

Address: #372, Industrial Area Phase I

Panchkula

Haryana

India

PIN 134112

Website: www.moodyint.com



Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..

I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.



Please guide me to select the best agency which will provide good preparatory training.



Regards



Prem Nautiyal

Mumbai.

PREM S NAUTIYAL


CELL : 9820313278



--
Click for exclusive coverage on the New Bajaj Pulsar 220 the fastest Indian bike
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2838] Re: CEA COURSE

Dear All ,
DNV Norway and DNV Singapore have complete arrangements for all failure analysis and fracture mechanics and ECA .Visit DNV web site www.dnv.com

Best Regards


----- Original Message -----
From: Ali Asghari
To: materials-welding@googlegroups.com
Sent: Tue, 28 Jul 2009 09:42:45 +0530 (IST)
Subject: [MW:2831] CEA COURSE

Hi all
does anybody have information about international certificates & organizations about failure investigation or critical engineering assessment and fracture mechanics?
 
regards.
 
 



--
Click for exclusive coverage on the New Bajaj Pulsar 220 the fastest Indian bike
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2839] Re: AWS-CWI best agency in INDIA

Dear Prem,
I suggest you that if you are planning to attend AWS for Overseas job opportunities then please think about CSWIP 3.1 welding Inspector.
main difference : AWS validity - 3 years.
                         CSWIP 3.1 - Validity 5 years
AWS membership compulsory. every year you have to pay.
CSWIP membership not compulsory.
Renewal - AWS = INR 22000/- after three years CSWIP 3.1 = INR 15,000/-

Choice is yours! - CSWIP 3.1 = Tata Projects limited.
and for Preparatory courses IANT ( Institute of Advanced NDT Technology)

Regards,
Nilesh


On Tue, Jul 28, 2009 at 4:33 AM, PREMSHANKARDUTTNAUTIYAL <prem_nautiyal@rediffmail.com> wrote:
Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278




--
Best Regards,

Nilesh Pathare

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2834] Re: 2827] AWS-CWI best agency in INDIA


Iwhat is the meninig of IQS
Thanks & Regards,

K.GANESAN
Quality Control
ISGEC / ISGEC John Thompson,
A-4 Sector-24 Noida-201301 (UP)
Tel. +91-120-2411175
Direct Tel. +91-120-2411175
Mobile : +91-9952166894

--- On Tue, 28/7/09, SLM <smahuri@lntecc.com> wrote:

From: SLM <smahuri@lntecc.com>
Subject: [MW:2829] RE: 2827] AWS-CWI best agency in INDIA
To: materials-welding@googlegroups.com
Date: Tuesday, 28 July, 2009, 9:20 AM

Yes, you have rightly heard.

 

Among the four listed agencies IQC is the best. As most of my friends have completed this course successfully through IQC only.

So you can opt for IQC.

 

 

Thanks and Regards,

 

Snehkumar L Mahuri

Regional Quality Manager

HC&P (Vertical)

 

M : 9428819849

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL
Sent: Tuesday, July 28, 2009 9:04 AM
To: materials-welding@googlegroups.com
Subject: [MW:2827] AWS-CWI best agency in INDIA

 

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278

</Table


 


"This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"


See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2833] Toughness Requirement for Dissimilar Weld

Your understanding is correct. It is exempted


From: Vivek Bhisade [mailto:vivek@tpr.grengg.com]
Sent: Tuesday, July 28, 2009 2:20 PM
To: materials-welding@googlegroups.com
Subject: Toughness Requirement for Dissimiller Weld

 

 

Dear All,

 

We have a  job ( hydro generator) material SA 387 Gr.11 CL 2 + SS347 ( clad) ,required impact testing at (minus)-18 Deg.C with energy value 33 J average (irrespective of MDMT ),having some nozzles (LWNR) material is SA 182 F 347.   

For  Welding Procedure Qualification of Dissimilar metals Nozzle to Shell joint ( P4 To P8) using electrodes by E309L , weld Impact test is required or not?

As per ASME SEC VIII Div 1 – UHA-51 (e) it is exempted ,

Please advise.

 

Thanks in advance.

 

 

 

 

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2835] Toughness Requirement for Dissimiller Weld

 

 

Dear All,

 

We have a  job ( hydro generator) material SA 387 Gr.11 CL 2 + SS347 ( clad) ,required impact testing at (minus)-18 Deg.C with energy value 33 J average (irrespective of MDMT ),having some nozzles (LWNR) material is SA 182 F 347.   

For  Welding Procedure Qualification of Dissimilar metals Nozzle to Shell joint ( P4 To P8) using electrodes by E309L , weld Impact test is required or not?

As per ASME SEC VIII Div 1 – UHA-51 (e) it is exempted ,

Please advise.

 

Thanks in advance.

 

 

 

 



 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2832] RE: 2831] CEA COURSE

Dear Ali,

 

If you are looking at an international company that undertakes failure investigations , you can count on TCR Engineering Services and our sister concern TCR Advanced Engineering based in India. We have done over 800 failure investigations, RLA and Condition Assessment on various metallic components related to almost all the engineering fields over past one decade. Please visit our website at www.tcreng.com to know more about our FA services.

 

Regards,

Rohit Bafna

Director - Global Sales

 

------------------------------------------

TCR Engineering Services (India)
TCR Arabia (KSA), TCR Kuwait

TCR Consulting FZC (UAE)

TCR Nigeria, TCR Malaysia

TCR World Inc. (USA)

India Tel: +91-983-353-0400

www.tcreng.com
Material Testing | Consulting | Inspection | NDT Services

-------------------------------------------

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Monday, July 27, 2009 11:13 PM
To: materials-welding@googlegroups.com
Subject: [MW:2831] CEA COURSE

 

Hi all

does anybody have information about international certificates & organizations about failure investigation or critical engineering assessment and fracture mechanics?

 

regards.

 

 



 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2836] Engg Course materials Online

Dear Friends

The IITs have taken up an initiative of starting online teaching and thus
> have started offering course materials online for every engineering
> stream.
> Many professors from all the IITs have provided course materials for each
> chapter and each subject..
>
> One has to register at the link provided below and can access the course
> material free of cost.
>
> Every Chapter has been described with diagrams and charts. Please spread
> this message to everyone, as many can benefit from this program taken up
> by the government and IIT.
>
> This is just a trial period going on and hence I request everyone to
> register at the link given.
>
> 1] Type the following address on internet explorer
> http://www.nptel.iitm.ac.in
>
> 2] Click on Courses and one can access any course material.
>
> Please spread the word, so that this initiative benefits as many Students
> as possible.
>
> Regards
>
> Prem Nautiyal
Godrej,Mumbai
>


PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2837] Re: 2827] AWS-CWI best agency in INDIA

HI All,
It all depends upon the tutor and the materials which he
gives during the class.

Regards,
Y.C.Shiva,
QA/QC Engineer,
Certified Inspector API 653,570, CSWIP 3.1, NACE CIP lev 2,
Doha Qatar.

On 7/28/09, SLM <smahuri@lntecc.com> wrote:
> Yes, you have rightly heard.
>
> Among the four listed agencies IQC is the best. As most of my friends have
> completed this course successfully through IQC only.
> So you can opt for IQC.
>
>
> Thanks and Regards,
>
> Snehkumar L Mahuri
> Regional Quality Manager
> HC&P (Vertical)
>
> M : 9428819849
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> PREMSHANKARDUTTNAUTIYAL
> Sent: Tuesday, July 28, 2009 9:04 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:2827] AWS-CWI best agency in INDIA
>
> Hi Friends
>
> I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course
> + Exam in the next couple of months. But in India there are 4 AWS approved
> agencies which conduct this AWS course.I am confused as to which agency i
> should select as i have to invest a huge amount of money... .
>
> 1)Industrial Quality Concepts
> Address: IQC Training & Services, Pte, Ltd
> Shivani Block -1, Ist Floor
> 40 East Coast Road
> Chennai, India 600041
> Telephone: 91-44-42158714/42158715/24451009
> Fax Number: 91-44-5215-8715
> Email: iqc.in.org@vsnl.com
> Contacts: Sundaran Baskaran
>
> 2)BETZ Engineering & Technology Zone
> Address: 49-Vellalar Street
> Near St Thomas Mount Railway Station
> Chennai - 600088
> INDIA
> Tel: 91-44-65364123/22441234
> TeleFax: 91-44-22441234
> Email: betzzone@vsnl.net
> Site: www.betzinternational.com
>
> 3)DASH Inspectorate
> Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
> Saffron Circle,Fatehgunj,
> Baroda-390002,Gujarat,India
> Phone: +91 265 2750116, 3017474
> Fax: +91 265 2788278
> Site: www.dashinspectorate.com
>
> 4)Agency: Moody ICL Certifications Limited
> Address: #372, Industrial Area Phase I
> Panchkula
> Haryana
> India
> PIN 134112
> Website: www.moodyint.com
>
> Hence can anyone guide me from their past experience as to which agency is
> the best. Please give your unbiased opinion..
> I have heard from all my colleagues that IQC,chennai is the best and most
> experienced in conducting CWI.
>
> Please guide me to select the best agency which will provide good
> preparatory training.
>
> Regards
>
> Prem Nautiyal
> Mumbai.
>
> PREM S NAUTIYAL
>
> CELL : 9820313278
> [http://sigads.rediff.com/RealMedia/ads/adstream_nx.ads/www.rediffmail.com/signatureline.htm@Middle]<http://sigads.rediff.com/RealMedia/ads/click_nx.ads/www.rediffmail.com/signatureline.htm@Middle?></Table
>
>
>
>
>
> ________________________________
> "This Message and its contents is intended solely for the addressee and is
> proprietary.Information in this mail is for L&T Business Usage only. Any Use
> to other than the addressee is misuse and infringement to Proprietorship of
> L&T ECC.If you are not the addressee please return the mail to the
> sender.L&T ECC DIVISION"
>
> >
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2831] CEA COURSE

Hi all
does anybody have information about international certificates & organizations about failure investigation or critical engineering assessment and fracture mechanics?
 
regards.
 
 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2830] old/model question papers for API 570 exam

Hi every body,

 

Can anyone send me old/model question papers for API 570 exam. I hope this will be useful for many aspirants.

 

Regards

 

Vinod

 



__________ Information from ESET NOD32 Antivirus, version of virus signature database 4283 (20090727) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2829] RE: 2827] AWS-CWI best agency in INDIA

Yes, you have rightly heard.

 

Among the four listed agencies IQC is the best. As most of my friends have completed this course successfully through IQC only.

So you can opt for IQC.

 

 

Thanks and Regards,

 

Snehkumar L Mahuri

Regional Quality Manager

HC&P (Vertical)

 

M : 9428819849

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL
Sent: Tuesday, July 28, 2009 9:04 AM
To: materials-welding@googlegroups.com
Subject: [MW:2827] AWS-CWI best agency in INDIA

 

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278

</Table


 



"This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2828] RE: 2827] AWS-CWI best agency in INDIA

IQC is the oldest one in India, and I have no comments on the rest, anyway don’t worry much as industry colleagues says this one is difficult to fail (sorry nothing to degrade this exam but its moral booster to all who ever is appearing), it just basic knowledge on welding fundamentals are required.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREMSHANKARDUTTNAUTIYAL
Sent: Tuesday, July 28, 2009 9:04 AM
To: materials-welding@googlegroups.com
Subject: [MW:2827] AWS-CWI best agency in INDIA

 

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278




 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2827] AWS-CWI best agency in INDIA

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:2823] Re: Safety Question

Hi Joel, its been a while since you taught my manufacturing processes class (the one we did semiautomatic SAW). I'm happy to help. The answers are below and my company is in the signature.
 
1. No
2. Heavy Fabrication
3. Indoor

Regards,

Dale Jones
Welding Engineer & CWI
Fisher Controls, Emerson Process Management
Marshaltown, IA 50158


--- On Wed, 7/15/09, Armstrong, Joel <JoelArmstrong@letu.edu> wrote:

From: Armstrong, Joel <JoelArmstrong@letu.edu>
Subject: [MW:2691] Safety Question
To: materials-welding@googlegroups.com
Date: Wednesday, July 15, 2009, 9:04 AM


All,

I work for LeTourneau Technologies and we build some of the world's largest front end loaders and jack-up drilling rigs.  Obviously, we're a heavy fabrication facility.

Our Safety department has been asked to investigate the need of wearing hard hats in all manufacturing areas.  This would include assembly, machining, heat treat, cutting, as well as welding.

Our GM of Fabrication and Assembly has asked me to get a survey of other companies' policies on the wearing of hard hats.

So, if you could respond and let me know the following.

1.  Does your company require manufacturing personnel to wear hard hats?
         

2.  What type of industry are you in
       a.  Heavy Fabrication
       b.  Sheet Metal / Automotive
       c.  Construction
       d.  Wholesale Trade
       e.  Cutting
       f.   Other (Please specify)

3.  Does your manufacturing/operations primarily take place... indoors or outdoors.

4.  What is the name of your company.

5.  What country is your facility located?


Also, if you have recently changed companies or know for sure the policies of a facility other than your current location, feel free to answer the survey from that point of view as well.

Thanks,

Joel Armstrong, CWI
Welding Engineer
LeTourneau Technologies
Member AWS B1 Committee


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...