The best thing is to select super duplex SS bolts - if for offshore applications.
They have sufficient strength and will not be subject to galvanic corrosion.
 
regards
Kristian


From: Vinayak Kale [mailto:Vinayak_Kale@lntenc.com]
Sent: 4. december 2009 10:27
To: materials-welding@googlegroups.com
Subject: Re: [MW:3789] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo Stainless steel flanges
Importance: High


depending upon process requirement , you can choose either power or xylene coating , this will have cost implication or one more way , go for Hot Dip Galvanizing or electroplating , which ever is affordable  



Thanks & Best Regards,

Vinayak Kale
E & C  DIv. QA & I , OGSP
Larsen And Toubro Ltd
Powai , Mumbai
vinayak_kale@lntenc.com
Ph No.+91- 67053805/3685
Fax No. +91-67054789
(M) - + 91 9892743803

Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...