<Security Level 2>                                                                                                                                                                                                                                                                                                                                                                                                                                
Many Licensor's specification specifies A193 B7 / 2H bolts for stainless steel flamges.
Use of galvanised bolt not seen at all for SS flanges.

Also note, A193 B7/2H bolts are not CS bolts. These are alloy steel bolts.

I did not understand the stage of your project . If youare planning to buy new one than buy ss bolts or can go for B16 / 4 bolts also.


Thanks & Regards,
Dhwani Desai.
TOYO - PLANNING & PIPING DEPT.
91-22-2573 7681.



"Pisat, R. R(ahul)" <Rahul.Pisat@akzonobel.com>

12/04/2009 02:33 PM

Please respond to
materials-welding@googlegroups.com

To
<materials-welding@googlegroups.com>
cc
Subject
[MW:3787] type coated Bolts carbon steel bolts ( A193 Gr. B7 ) fo         Stainless steel flanges





Hello all,

Please recommend me the type of coated carbon steel bolts ( A193 Gr. B7 ) to use with stainless steel flanges.
I am sure no to apply galvanised bolts with SS flanges.

Our construction team is worried about the rusted of the carbon steel bolts to be apply with stainless steel flanges.

Please reply your recommendation for type of coating for bolts ?

Kind regards

Rahul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...