Tuesday, December 1, 2009

Re: [MW:3782] hydrotest b31.1

Hi,
As per para 345.3,B31.3
All joints may be primed
and painted prior to leak testing unless a sensitive leak
test is required.
Regards,
Mohd. Sadique

On Tue, Dec 1, 2009 at 2:24 AM, John Lock <j.lock@pacificdrilling.com> wrote:

Primer coats are permitted

 

Best regards,

 

John Lock

Quality & Classification Engineer

Pacific Deepwater Construction Ltd

cid:image002.jpg@01CA4F2E.75D71400

Cellular.                 +82 (0)10 4693 6282

Office Tel.              +82 (0)55 631 9071

Office Fax.             +82 (0) 631 7499

E-mail                    j.lock@pacificdrilling.com

P Before printing I think about the environment

 

From: daniel iordache [mailto:daniel.iordache@gmail.com]
Sent: Monday, November 30, 2009 11:39 PM
To: materials-welding@googlegroups.com
Subject: [MW:3771] hydrotest b31.1

 

Hi, 

 

I have a strange situation about Hydrostatic Test ......

 

Until now we used to let all welds of piping system no painted........

 

now our client read in B31.3 and open the discussion that in code is wrote that is allowed to paint the welds before hydrostatic test......

 

What do you think about that?????

 

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...