Wednesday, December 9, 2009

[MW:3807] Welding of P5A & P5B Material

Can any body inform about the …..

For the welding of SA 335 Gr. P91 (PNo-5B, Group No-2) Material………
1) What is the Preheating Temperature?
2) What is the Post heating Temperature & Time ?
3) PWHT is require or not ?
4) While welding (GTAW) Backing is require if yes, then Argon is OK ?

For the welding of SA 335 Gr. P22 (PNo-5A, Group No-1) Material………
1) What is the Preheating Temperature?
2) What is the Post heating Temperature & Time ?
3) PWHT is require or not ?
4) While welding (GTAW) Backing is require if yes, then Argon is OK ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...