Skip to main content

[MW:3467] Re: 3448] Re: Qualification of cladded base metal

Hi Hegde and Ibrahim,

Yes i want to weld P5A claded with 316L to 316L plate. Based on your explanation
s, i prefer to choose item i. For your info there is no clad restoration. But how about if clad restoration is require. Is it i need to qualify overlay procedure. Thank a lot guys for your valuable explanation.

Regards
tong2je

On Thu, Oct 8, 2009 at 11:58 AM, PB HEGDE <hegde.pb@isgec.com> wrote:

Hi !Tong

From your  query I presume  You want to weld P5A claded plate to SS316L plate.

Such case

You require to qualify PQR  i) Butt weld of  SS 316L to P5A i.e. P8 to P5a using NiCrMo3 with require PWHT as per code UCS 56

ii) option2  Butter the P 5A  with NiCrMo3 carry out the PWHT as per code later weld with the same with P8 to buttered P5A  but w/o PWHT This will be job specific PQR

Hope there is no clad restoration on SS portion

 

Regards

 

Hegde

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim
Sent: Wednesday, October 07, 2009 7:51 PM
To: materials-welding@googlegroups.com
Subject: [MW:3448] Re: Qualification of cladded base metal

 

Hi tong,

 

You have to qualify the procedure as the same configuration of production. For cladded and buttered configuration you have to make the same test coupon and weld. You have to confiy the chemistry also at the root.

 

Regards,

Ibrahim

2009/10/6 tong tong <tong2je@gmail.com>

Dear All,

 

I have one query regarding welding qualification of cladded base metal. Our first base metal is Stainless steel 316L to weld with second base metal P5A cladded with Stainless steel 316L. A layer of ENiCrMo-3 was buttered on bevel of second base metal by other. As i know a layer of ENiCrMo-3 act as barrier layer. The problem is how to qualify the welding procedure on stainless steel 316L to P5A cladded with Stainless steel 316L. Is it i need to qualify  P5A cladded with Stainless steel 316L or Stainless steel 316L to inconel ENiCrMo-3 or Stainless steel 316L to Stainless steel 316L procedure. I really need your advice and expertise. What is the best practice or code requirement on qualification of cladded base metal. Advance thank for your kind cooperation and really appreciated

Regards

Tong2je

 




--
Thanks & Regards
Muhammed Ibrahim PK






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...