Sunday, October 4, 2009

[MW:3426] Re: UT testing-1

Rajaneesh,
Please take it on a word format file and give dimensions, identify N1 also. Then comments can be given on the figure itself.
.Shashank Vagal

--- On Sun, 4/10/09, Rajneesh Gaur <rajneeshgaur@gmail.com> wrote:

From: Rajneesh Gaur <rajneeshgaur@gmail.com>
Subject: [MW:3414] UT testing
To: materials-welding@googlegroups.com
Date: Sunday, 4 October, 2009, 3:32 PM

Good afternoon,

I need to check the soundness of the W3 weld as indicated in the attached drawing extract by using UT as per client's requirement. Can someone guide me if it is possible, and if it is possible, then can someone tell me how.

This is a 4" nozzle to shell weld with RF pad welded on it.

 

Regards

Rajneesh





Try the new Yahoo! India Homepage. Click here
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...