[MW:3417] RE: 3414] UT testing

Dear Rajneesh

 

                UT testing is possible for the joint which u asked. But the efficiency or accuracy we cant able to say. It depends upon the technician who is doing. This type of joint UT can be done from inside and by Half Skip method.

 

Regards

P.Asok Kumar

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rajneesh Gaur
Sent: Sunday, October 04, 2009 1:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:3414] UT testing

 

Good afternoon,

I need to check the soundness of the W3 weld as indicated in the attached drawing extract by using UT as per client’s requirement. Can someone guide me if it is possible, and if it is possible, then can someone tell me how.

This is a 4” nozzle to shell weld with RF pad welded on it.

 

Regards

Rajneesh


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...