[MW:3409] Re: application of SS Flux cored wire for GTAW, SFA 5.22

Dear Mr Raghuram,
I don't understand GTAW with Flux cord wire, it should be FCAW.
My suggestion is to do it with gas purging for better penetration and
fast production.

Or Use SMAW process because i have qualified so many welders in SMAW
with better penetration. or use combine process SMAW for Root and Hot
Pass Filling and Capping with FCAW.

On Oct 2, 5:24 am, ikaria73 <ikari...@hotmail.com> wrote:
> JZ,
> You are correct.  If proper training is not conducted with the STT
> process, the type of defects you experienced will be common.  Lincoln
> developed STT in the late 1980s and has been a proven process on in-
> house and cross-country pipe but proper training is important.
> Fortunately most of Lincoln's technical sales representatives
> graduated from college as engineers and have been trained to properly
> weld with STT.  Hopefully they can help.
>
> Regards
>
> On Sep 25, 3:08 pm, Jeremy Zibin <jzi...@yahoo.com> wrote:
>
>
>
> > Something to add to this GMAW discussion:
> >  
> > I've performed quality control work and inspection at a large piping fabrication shop where they were using mainly STT GMAW because of the high production rates inherant with this welding process.  There were mainy issues with lack of fusion or porosity in the root and the quality of welds being of concern.  I've later talked with welding engineers and consultants who have said that any type of GMAW process, whether its STT or other, will be susceptible to these types of defects, especially in the root of the weld. 
> >  
> > I'm not saying it's impossible to perform but the welders must have very good training with the capabilities of the machines and they must be aware of the difficulties in root welding otherwise you will have a large quality "headache" on your hands.  One possible solution is to grind away any weld starts that are suspect at having defects before welding over with the following passes (the welders at the shop I was working did not do this from what I could see and hence, likely propagated the problem).
> >  
> > Regards,
> >  
> > J.Z. 
> > Materials & Welding Engineer
>
> > --- On Thu, 9/24/09, Vishal Mehta <v...@supertechservices.in> wrote:
>
> > From: Vishal Mehta <v...@supertechservices.in>
> > Subject: [MW:3309] Re: application of SS Flux cored wire for GTAW, SFA 5.22
> > To: materials-welding@googlegroups.com
> > Received: Thursday, September 24, 2009, 9:24 PM
>
> > Yes, STT is a good option only if you could use GMAW process. And its worth an investment only if such jobs are regular.
>
> > Besides STT, even Miller Electric has developed their patented technology RMD - Regulated Metal Deposition. Machine Model is Pipepro 450. Its somewhat similar to STT and a little more to offer. checkwww.millerwelds.com
>
> > Regards
>
> > VISHAL
>
> > On Fri, Sep 25, 2009 at 8:54 AM, vipin george <vipingeor...@gmail.com> wrote:
>
> > Dear Bathula,
> >  
> > A new process is developed by Lincoln STT(Surface tension transfer) it's GMAW process with short circuit transfer.It's good for piping applications.Check Lincol electric.
>
> > Regards,
> > vipin
>
> > On Tue, Sep 22, 2009 at 12:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bath...@ticb.com> wrote:
>
> > Dear members
> > We have typical vessel (site assembly), where backing gas arrangement could not be done for a stainless steel joint due to Safety (confined space), as well as space constraint.
> > One of the options will be using flux cored wire for GTAW.
> > Please share your view on these consumables for root pass of GTAW Stainless steel; where backing gas application is impractical, any body used these consumables?
> > Kobleco is manufacturing these wires under TGX series, any other manufactures who has similar product for this application?
>
> > --
> > SUPERTECH SERVICES LTD
> > Plot A-253, Road 30B,
> > Wagle Indl Estate,
> > Thane W 400 604
> > Maharashtra, India
> > Tel: +91-22-25826190/91
> > Fax: +91-22-25826189
> > Email: v...@supertechservices.in
> > Web:www.supertechservices.in
>
> >       __________________________________________________________________
> > Get a sneak peak at messages with a handy reading pane with All new Yahoo! Mail:http://ca.promos.yahoo.com/newmail/overview2/- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...