[MW:3408] prequalified wps

Hi FRIENDS
is it possible to write a prequalified wps for ST37 according AWSD1-1?(THIS MATERIAL NOT LISTED IN TABLE 3-1,BUT HAVE SIMILLAR COMPOSITION WITH SOME LISTED )
REGARDS.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...