[MW:3402] RE: 3373] filler wire for copper

You can use ASW A5.7 ERCU electrode

THANKS

@Mohammed Fathi

Senior QC/QA Engineer

Arab Steel Fabrication Co. ASF (Elsewedy)

( Tel #: +2 015 4111 70 ~ 75 ext.: 190

r Fax #: +2 015 4111 76

) Mob#: +2 0184775115

* E-mail : mfathi@elsewedysteel.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of gajjalla surya
prakash
Sent: Wednesday, September 30, 2009 8:17 AM
To: materials-welding@googlegroups.com
Subject: [MW:3373] filler wire for copper


dear all ,

can any one sujjest me the filler wire for GTAW process for weld 12mm
thk Pure copper to copper plate(99.3%)

--
With regards,

Surya Prakash Gajjalla
ASSOCIATED ENGINEERING SERVICES
3-5-944/220-221 panchavatimall narayanaguda hyderabad india 500029.

www.aesinspections.com
0091 9885162668

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...