For less than 3.2mm thick, AWS D 1.3 Structural welding code sheet steel is applicable.
 
Regards
Loni

On Sat, Sep 19, 2009 at 6:28 AM, raw <rohit30584@gmail.com> wrote:

Hi everyone out there,
Can anyone of you clear my query that in AWS D1.1,we talk about
thickness greater than 3.2mm and not less than that.
Thanks,
Rohit Rawat(QA)




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...