[MW:3242] Re: Shelf life of Low hydrogen electrodes

There is no such conditions in code , but to avoid any quality issues or rejection ,you may check the electrodes for any damages of the coating and if there is no damages to the coating and no absorption of moisture ,just rebake the electrodes and use it. Verifiy if  there is some conditions put by client specifications or manufacturer.
Best Regards,
Francis Lobo

----- Original Message -----
From: Ravindra T
To: materials-welding@googlegroups.com
Sent: Thu, 17 Sep 2009 15:28:01 +0530 (IST)
Subject: [MW:3238] Shelf life of Low hydrogen electrodes

Dear All

 

Our contractor has brought low hydrogen electrodes (E 7018 & 8018) which are manufactured in 2007 for welding station piping in one of our intermediate pump station of our cross country pipeline project. I would like to know whether these electrodes can be used now?. Is there any reference in ASME code regarding the expiry/ shelf life of Electrodes?


 

Please advise me in this regard.

 

Thanking you all in advance

 

Ravindra

Senior Project Engineer



--
Click for exclusive coverage on the New Bajaj Pulsar 220 the fastest Indian bike
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...