Please refer the Code what you are using for design and manufacturing.
eg ASME Sec I, VIII, AWS D1.1 or others...


Thanks
Senthil

On Sep 15, 3:20 pm, sandy kumar <sandy001...@gmail.com> wrote:
> Can anyone please provide me following details
>
> 1.       How to calculate preheat & Post heat for welding?
>
> 2.       How to calculate cooling rate for welding?
>
> 3.       How to know heat input effect on steel (Tempered steel) mean how to
> know how much max. heat required for any material specially where notch
> toughness required?
>
> Please do the needful.
>
> Best regards
> Sandeep Kumar

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...