[MW:3213] Re: 9cr-1Mol

No you can't do it; should do it by the actual material only...

Do you have qualification for buttering? How did you arrive that WPS?

Thanks
Senthil

On Sep 8, 6:09 pm, Harikumar Dayalan / ZS Saudi PED QA/QC
<hariku...@zamilsteel.com> wrote:
> Dear Friends
>
> I need to qualify procedures for P5B (9Cr-1MoL) material urgently, at
> present I don't have any material in stock
>
> Since the preheat, interpass, interpass stress relieving and post weld
> temperature for P5B are too maintained strictly.
>
> is the procedure qualification is  possible by buttering? Did the secIX
> and Sec VIII Accepts.
>
> Did anybody done it, if so how about the mechanical test results.
>
> Regards
>
> Harikumar Dayalan
>
> <mailto:hariku...@zamilsteel.com>    
>
> ---------------------------------------------------------------------------­-----------------------------
> Disclaimer: This email and any files transmitted with it are confidential
> and intended solely for the use of the addressee(s) named herein. If you
> are not the intended recipient or addressee, you should not use, disseminate,
> distribute, copy or alter this email. Any views or opinions presented in this
> email are solely those of the author and might not represent those of "Zamil
> Industrial" and or its units.
>
> Warning: Although reasonable precautions have been taken to ensure no viruses
> are present in this email, the company cannot accept responsibility for any
> loss or damage arising from the use of this email or attachments. If you have
> received this electronic mail message in error, please contact the sender directly.
>
>  image001.gif
> 1KViewDownload

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...