ASME Sec-VIII Div.1 , UCS-56 (f) gives the restrictions on P No.1 & P No.3 weld repair by SMAW process ( UCS-56 (f)(4)(a) ) , but for other materials they didn't give ant restrictions.
hence you can convince your client to do the repair by GTAW process.
Also filler weld will not be such problem logically.
 
Regards,

On Wed, Sep 9, 2009 at 4:41 PM, prabhakar s <prabhakars84@gmail.com> wrote:
Hi,
 
We have to repair a fillet weld joint which is welded by SMAW process. Material is SS (A312 Gr316L). Can we do the repair with GTAW? Is it allowed as per any code? Please give me the reference also.
 
 
We have a WPS for GTAW process on SS Material (A312 Gr316L).  
 
Regards
Prabhakar. S





--
Sukamal


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...