[MW:3148] RE: 3143] 9cr-1Mol

No such short cut is allowed in the code
________________________________________
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Harikumar Dayalan / ZS Saudi PED QA/QC
Sent: Tuesday, September 08, 2009 6:39 PM
To: materials-welding@googlegroups.com
Subject: [MW:3143] 9cr-1Mol

Dear Friends

I need to qualify procedures for P5B (9Cr-1MoL) material urgently, at present I don't have any material in stock

Since the preheat, interpass, interpass stress relieving and post weld temperature for P5B are too maintained strictly.

is the procedure qualification is  possible by buttering? Did the secIX and Sec VIII Accepts.

Did anybody done it, if so how about the mechanical test results.


Regards
Harikumar Dayalan
  

Filtered by Hosted Filtering

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...