you won't find any code or standards that says not to use pneumatic testing... but if you calculate the energy stored on testing your 10-12" pipe, it will be huge... I mean really HUGE! so safety takes priority... if anything goes wrong, I wish nobody is even near the pipe!
 
As already recommended... try to convince the client (if that is the origin of the idea) for a full NDT and service test. It is safer!


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of daniel iordache
Sent: 08 September 2009 07:57
To: materials-welding@googlegroups.com
Subject: [MW:3137] hot-oil traced line

hello Friends
 
we have in project 10-12" bitumen line .......these lines are accompanied by hot-oil traced line 1" sch 40....maximum pressure for those line are 30 psi.....due the complexity of network ....i want to test line instead of hydrostatic ...pneumatic at 90 psi ... ....there is any restriction..? Most of people said is avoid to do pneumatic test ...by code ....i did not find any ....
 
please advice

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...