Dear Friends

 

I need to qualify procedures for P5B (9Cr-1MoL) material urgently, at present I don’t have any material in stock

 

Since the preheat, interpass, interpass stress relieving and post weld temperature for P5B are too maintained strictly.

 

is the procedure qualification is  possible by buttering? Did the secIX and Sec VIII Accepts.

 

Did anybody done it, if so how about the mechanical test results.

 

 

Regards

Harikumar Dayalan

  

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...