[MW:3138] RE: 3137] hot-oil traced line

Avoid due to safety reasons, please see the attachment. Or convince your client with additional NDT along with very low pressure pneumatic test followed by service test.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of daniel iordache
Sent: Tuesday, September 08, 2009 12:27 PM
To: materials-welding@googlegroups.com
Subject: [MW:3137] hot-oil traced line

 

hello Friends

 

we have in project 10-12" bitumen line .......these lines are accompanied by hot-oil traced line 1" sch 40....maximum pressure for those line are 30 psi.....due the complexity of network ....i want to test line instead of hydrostatic ...pneumatic at 90 psi ... ....there is any restriction..? Most of people said is avoid to do pneumatic test ...by code ....i did not find any ....

 

please advice


--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...