[MW:3120] Re: CS (A106 GR B) TO AS (A 335 P11)

Dear Mano
can you describe the service condition of the joint?(max temp  & severity of corrosive environment)
regards


From: Manoharan Kalimuthu <kmanoharan68@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, September 4, 2009 1:21:58 PM
Subject: [MW:3117] CS (A106 GR B) TO AS (A 335 P11)

Dear All,
                      Here in our project we have A106 GR B to A335 P11 Dissimilare welding ,Can any on suggest the filler wire and Electrode?
Is it possible to use ER309 and E309.
Regards
Mano
 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...