[MW:3114] Re: Hydrotest for high pressure piping

Romove the valve for the pressure test, (it should have been pressure tested previously)
 
you can then use this valve access point to pressurize and record the pressure during testing,
 
regards,
 
Nick Davies
 
 
 


 
On Thu, Sep 3, 2009 at 6:47 PM, tong tong <tong2je@gmail.com> wrote:
Dear Nick Davies,
As i mentioned before, there are no isolation point. This line has 1 welded valve. We not sure whether this valve can withstand the test pressure and possiblity of valve leak. 

On Thu, Sep 3, 2009 at 12:12 AM, Nick Davies <nickdavies3@gmail.com> wrote:
Tong,
 
you should perform a pressure test on the pipeline, do you have valves in the line? there must be some tie-in points or valves in the line?
 
Nick Davies

On Wed, Sep 2, 2009 at 6:19 AM, tong tong <tong2je@gmail.com> wrote:
Dear All,
I have one tie-in point. The material is SA 312 TP316L. The test pressure is 350 bar and operating pressure is 250 bar. The big problem is there are no isolation point so hydrotest can't be performed on it. When I refer to API 570, clause 8.2.6 stated that when a pressure test is not necessary or practical, NDE shall be utilized in lieu of a pressure test. Due to this line is high pressure, is it enough only perform the NDT ? How suppose i do to convince our management level regarding integrity of the weldment ? Please help me. Thank in advance and you cooperation is highly appreciated 
Regards
Tong2je






--
Regards,

Nick Davies









--
Regards,

Nick Davies

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...