Thursday, September 3, 2009

[MW:3104] Re: Hydrotest for high pressure piping


Dear Tong,
 
In addition to the Radiogrpahy at the end, carry out Dye penetrant test during Edge preparation , After Root, After 50% of the welding and after the final welding, inorder to ensure the integrity of the joint. This is the universally being followed in all industries.
 
Regards,
 
Siva


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...