Wednesday, September 2, 2009

[MW:3098] Re: PQR FOR A570Gr40 and A570 Gr36

Hi,
As per Asme sex-IX there is no P no. or G no. for this material,
This material asigned in UNS number  with S no and G no.
As per sec IX  clause QW-420.2 if you take PQR on any grade 36 will cover for S no and G no in that particular UNS No.
 
Mohan.

On Sun, Aug 30, 2009 at 11:47 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
both belongs to S#1 Gr#1 (refer QW 422 of ASME BPV Section IX)
yes, you can use since both belongs to same grouping

On Sun, Aug 30, 2009 at 9:46 AM, Samimi Mottagi, Alireza <Samimi@mapnagenerator.com> wrote:

HI

Kindly please inform me that I have two material  A570Gr40 and A570 Gr36 and I want to know where in Asme Standard I can find the P no. and Gr no. of them and according to Asme if I take a PQR on A 570 Gr 36 is it cover the A570 Gr 40 or not. Please give me the coorect address of standard.

thanks






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...