[MW:3097] RE: 3096] Re: API 934 materials suppliers

Arcelor Mittal, Industeel in US and Dillinger from Germany are the major suppliers. In addition to X and J factor take care of simulated HT and testing at min and max PWHT conditions while ordering.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kural
Sent: Wednesday, September 02, 2009 3:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:3096] Re: API 934 materials suppliers

 

J

 

you can specify the X bar and J factor requirements in your purchase spec and there are quite few compannies who can supply . These are usually run in the mill on order basis.Any reputed manufacurer should be able to do it.

 

JSW, japan one among them


Regards

 


 

On Tue, Sep 1, 2009 at 9:00 AM, J <jhenning@deltak.com> wrote:


I would like to know if anyone knows of material manufacturers or
suppliers that are commercially supplying plate with certification to
API 934C (1-1/4Cr 1/2Mo).  If suppliers, prefer those in or with US
offices.

thanks.




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...