i.e. slightly acidic pH), LTCS A333-6 pipe material, 2 mm CA
When more acid is likely (i.e. for acid solution or acid + caustic
mixture upstream of neutralization vessel when neutralization is not
complete), PTFE lined LTCS
Please note that LTCS is used because of ambient temperature in
Kazakhstan during winter.
Regards,
Rajavelu
On Aug 16, 1:24 am, l l <lkthakur2...@yahoo.com> wrote:
> Sir,
> spent caustic trearment plant having always leakage in treated spent caustic (with pH 5 to 9 ) line , while piping has been made by cs material , we want to replace the piping with suitable material and low cost while line pressure is 6 kg/cm2.
> kindly sugest the material with details.
>
> Regards
>
> Lalit Kumar
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/