The clorine content should be 20 ppm below... in water.......
Regards,
Y.C.Shiva,
QA/QC Engineer,
Doha Qatar
On Sun, Aug 16, 2009 at 6:18 AM, Ali Asghari <asghariali@rocketmail.com> wrote:
dear all freindscan you share your expriences about the amount of CL in water that used for hydrostatic testing of st.st?because in somewhere i see 25 ppm and another 50ppm is mentioned.which correct & why?regards
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---