On Sun, Aug 2, 2009 at 9:25 AM, ARI <ariv2k@gmail.com> wrote:
Dear Javed, Enclosed the details,Regards,
Nom. Fig.Size
Ins. (mm)
Bolting
No. x Dia.
Ins.
Rec.
Bolt Stress
lb/in2
Torque lbf.ft. (Nm)
Bolt Lubricant
Molykote 1000 (µ = 0.11)
36 (900)
20 x 3 ½" UN8
45,000
15983
(21670)
On 8/2/09, Mohammad Javeed <mmubasharjaveed@gmail.com> wrote:Dear all
Have a nice day
I need your help about one query regarding torque value. We have a one flange joint of dia 36" RF CL. 900 material A350-LF2.and bolt length is 800mm. As per our client requirement this tightening should be done with hydraulic tensioning system. So what should be the torque value for this flange?
Thanks
M javed
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments