Dear Members,
We have a welded the nozzles to shell 40mm thick.As per API 650 we have done PWHT of full assembly in the furnace.After PWHT in MPI we found some indication which is going more deeper than 4mm.Can anybody tell me whether PWHT is required to be done once again after this repair.API 650 gives requirememts only for stress relieving but not for repair.Can i apply ASME SEC VIII div 1 UCS 56 Subclause 9(F)(2) for this repair.
regds
--
Nilesh Parsekar
Sr QC Co-ordinator
Exterran Belleli Energy
Fujairah - Sidem
Mobile - 0506561785
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---