Gentleman,
If I may ask how is PWHT accomplished in this case, is it with a furnace, induction heating or with a gas torch?
Many thanks
Roger H.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of G Padmanabhan
Sent: Monday, July 13, 2009 7:46 AM
To: materials-welding@googlegroups.com
Subject: [MW:2677] Re: service wise requirement for PWHT
Hi sadique,
Designer has to specify pwht requirements.For example CS in amine service required PWHT irrespective of thickness.Even support welding required pwht.
It depends upon how material will react to service condition.
On Sat, Jul 4, 2009 at 5:47 PM, Sadique Sheikh <sadiq.mech@gmail.com> wrote:
Hello to all of you.
Dear friends I have one query which I like to ask you
As per table 331.1.1 of ASME B31.3,it is mentioned here the
requirement of PWHT as per thickness and tensile strength for
mentioned materials.But how can I get information according to service
vise? This requirement is depend on project specification but i want
to know that, on which basis they calculate this requirement? Which
factors will consider during calculation? and how this factors affect
during service?
Regards
SADIQUE
--
With Warm regards,
G.Padmanabhan
00967771103169
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments