One Seagoing vessel has a repair to be carried out on a pipe.
The flange of the pipe is welded and the flange is broken in parts.
The only sketchy information available is the material of the flange is supposed
to be "16 MN (or 16 mn ??) steel". The vessel is in a remote port and material testing lab
is not available in the port. Can the members throw some light as to what this material
may be and what welding process / consumables may be used??
Consumables can be sent by road or similar transport, and the marine repair yard should be
having standard welding equipment for SMAW and possibly also for MIG/MAG & GTAW.
Thanks in Advance!
G. A. Soman
Principal
DON BOSCO MARITIME ACADEMY
Premier Automobiles Road,
Kurla West, Mumbai 400070
Tel: (022) 2504 1585 / 2018; 25036344. Fax: (022) 2504 0682
Email: donboscomarine@vsnl.net
Website: www.dbma.in
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments